BaGa4Se7 Crystal Options
′�?, which has a frequency of 295 cm−one, is attributed to the stretching vibration of Ga–Se bonds. The 2-phonon absorption from the 295 cm−1 phonon corresponds into the crystal IR absorption edge, rather then the residual absorption peak. Density practical theory computations clearly show the residual absorption in the BGSe crystal origi